Quick Answer
Last updated: September 2026. The film datasheet decides more of your line’s success than the machine does. Here is every field that matters, decoded.
Datasheet fields that matter
| Field | Looks like | Why it matters |
|---|---|---|
| Total gauge | 60 µm (235 ga) | Seal speed, stiffness |
| Structure | PET//alu//PE | Barrier + sealant logic |
| Sealant type | PE / CPP / ionomer | Seal temp range, contamination tolerance |
| Seal initiation (SIT) | 90 °C | Lower = faster, wider window |
| OTR | 1.5 cc/m²/day | Oxygen barrier (coffee needs <2) |
| WVTR | 0.5 g/m²/day | Moisture barrier (snack critical) |
| COF | 0.25 outside / 0.35 inside | Machine slip; too low = tracking chaos |
| Treatment level | 38–42 dynes | Print/ink adhesion |
| Roll width tolerance | ±1 mm | Pouch format accuracy |
| Core | 76 mm (3″) | Machine mandrel match |
Common spec traps
**Gauge traded for price** — 5 µm thinner film costs 8% less and doubles seal leaks.
**OTR quoted at 23 °C/0% RH** — real cold-room performance is worse; ask for conditioned values.
**COF both sides listed as one number** — inside/outside differ; outside needs machine slip, inside needs product slip.
FAQ
Can I run a cheaper film on the same machine?
The machine runs it — at 5–15% slower with more rejects. The film saving rarely survives the speed loss.
What single test predicts machine problems?
A COF check on both sides against your machine’s spec — takes minutes, prevents weeks of tracking hell.